MEMSnet Home: MEMS-Talk: Looking for vendors/services for HDP-CVD of Silicon Nitride
Looking for vendors/services for HDP-CVD of Silicon Nitride
2009-04-17
Harshal Surangalikar
2009-04-17
Pat Kayatta
2009-04-20
Glenn Silveira
Looking for vendors/services for HDP-CVD of Silicon Nitride
Glenn Silveira
2009-04-20
Harshal,
HDP-CVD silicon nitride provides great gap fill with less hydrogen content
wet etch resistance to HF not so much
HF resistant PECVD films
(a)SiCN
(a)SiC
(a)Carbon
(a)Si
Best regards'
Glenn

-----Original Message-----
From: Harshal Surangalikar [mailto:[email protected]]
Sent: Friday, April 17, 2009 12:10 PM
To: [email protected]
Subject: [mems-talk] Looking for vendors/services for HDP-CVD of
SiliconNitride


Hello,

I am looking for services/vendors in the area of "high density plasma"- CVD
(HDP-CVD) of Silicon Nitride films.

The motivation to go for HDP-CVD is to get higher wet etch resistance
(BOE/Conc. HF) than that provided by the PECVD films. If any info/references
are available on improving wet etch resistance of PECVD films, that will be
very helpful as well.

Thank for the time and best regards,
Harshal Surangalikar.

Sr. MEMS Process Engineer
Fortemedia
Cupertino, CA



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
University Wafer
Nano-Master, Inc.