MEMSnet Home: MEMS-Talk: Bearing holes in pyrex/glass wafers
Bearing holes in pyrex/glass wafers
2009-05-01
김태진
2009-05-01
Mehmet Aykol
2009-05-01
Kirt Williams
2009-05-02
Brian Stahl
2009-05-02
[email protected]
2009-05-02
Xiaoguang Liu
2009-05-02
Jackgong Hotmail
2009-05-02
HENRI FLECHNER
2009-05-03
Jackgong Hotmail
2009-05-04
Fei Wang
2009-05-04
Robert MacDonald
2009-05-06
김태진
2009-05-04
%Mihaela Carp
2009-05-02
HENRI FLECHNER
2009-05-03
tarun mudgal
2009-05-05
Jackgong Hotmail
2009-05-04
Tomblin, Graham
Bearing holes in pyrex/glass wafers
Xiaoguang Liu
2009-05-02
Hi Jim
Can the abrasive powder blasting be done in house or you send it out
to some service providers?
Thanks,
Leo

On Fri, May 1, 2009 at 11:19 PM,   wrote:
> TJ,
>
> I always liked micro abrasive powder blasting for quick turn prototype work.
>
> Jim
>
>

--
Xiaoguang "Leo" Liu
Birck Nanotechnology Center,
Purdue University,
1205 W.State Street, West Lafayette, IN, 47906 USA
[email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
The Branford Group
Tanner EDA by Mentor Graphics
Nano-Master, Inc.