Bearing holes in pyrex/glass wafers
2009-05-01
김태진
2009-05-01
Mehmet Aykol
2009-05-01
Kirt Williams
2009-05-02
Brian Stahl
2009-05-02
[email protected]
2009-05-02
Xiaoguang Liu
2009-05-02
Jackgong Hotmail
2009-05-02
HENRI FLECHNER
2009-05-03
Jackgong Hotmail
2009-05-04
Fei Wang
2009-05-04
Robert MacDonald
2009-05-06
김태진
2009-05-04
%Mihaela Carp
2009-05-02
HENRI FLECHNER
2009-05-03
tarun mudgal
2009-05-05
Jackgong Hotmail
2009-05-04
Tomblin, Graham
Bearing holes in pyrex/glass wafers
Jackgong Hotmail
2009-05-02
I also have the same question. But I want to drill a array of holes through
glass or any other transparent(to visible light) materials and the diameter
is around 400 micron. Hope some one can help us.

Gong

--------------------------------------------------
From: "김태진" 
Sent: Friday, May 01, 2009 3:31 PM
To: 
Subject: [mems-talk] Bearing holes in pyrex/glass wafers

> Hi all!
>
> I'm trying to think of a way to make a 2mm diameter through hole in a
> pyrex wafer.
>
> I thought of etching the hole with DRIE, but thought it was inefficient
> and time consuming.
>
> It also seems that I can't use conventional drilling machines to bear
> holes in the pyrex as the substrate is to brittle.
>
> Does anyone know how to drill holes in pyrex/glass wafers?
>
> The features don't have to be too accurate..
>
> Thanks!
>
> TJ
>
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Addison Engineering