Hi Ben

I am always do electroplating as thick as 20um. I thick you can try
50um-100um. Also, the thickness of electroplating is depend on the stress of
the metal.

Thanks
Ning

2009/5/25 Ben Pepin 

> Hello,
>
> I am an undergraduate research student at Mizzou and was wondering how
> thick
> of a coat you can achieve from electroplating? I am trying to get as thick
> of a coat as possible and would appreciate any tips or suggestions.
>
> Thanks,
> Ben Pepin
> [email protected]
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Addison Engineering
MEMS Technology Review