electroplating thickness
Phillipe Tabada
2009-05-26
Hi Ben,

   If it meets your needs you can look into the LIGA process which can produce
thickness between microns to several millimeters.

Phil

> Date: Mon, 25 May 2009 12:21:14 -0500
> From: [email protected]
> To: [email protected]
> Subject: [mems-talk] electroplating thickness
>
> Hello,
>
> I am an undergraduate research student at Mizzou and was wondering how thick
> of a coat you can achieve from electroplating? I am trying to get as thick
> of a coat as possible and would appreciate any tips or suggestions.
>
> Thanks,
> Ben Pepin
> [email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation