A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Lift- off Ti/Pt
Lift- off Ti/Pt
2009-08-20
Shah, Forum N
2009-08-20
Ruiz, Marcos Daniel (SENCOE)
2009-08-21
Huihang Dong
2009-08-21
DongJuan Xi
2009-08-21
Xiaoguang Liu
2009-08-21
Huihang Dong
2009-08-21
Brad Cantos
2009-08-22
Xiaoguang Liu
2009-08-22
Wilson, Thomas
2009-08-22
Brad Cantos
2009-08-21
mikas remeika
2009-08-22
Wilson, Thomas
2009-08-22
Brad Cantos
Lift- off Ti/Pt
mikas remeika
2009-08-21
The time it takes for the liftoff to occur depends on if you're using
an ultrasonic bath or not.

With ultrasonics it should be a matter of a few minutes (and contrary
to what some people say, ultrasonic treatment does not necessarily
damage fine features), whereas without ultrasonics it seems to be
common to leave the sample overnight for liftoff, however in my
experience, lifoff without sonication is very unreliable.

On Thu, Aug 20, 2009 at 2:33 PM, Shah, Forum N wrote:
> Hello All,
>
> I am sputtering a 250 Angstrom adhesion layer of  Ti and 1500 angstrom
adhesion layer of Platinum.
>
> Can someone tell me how long does it take for the lift - off to occur if the
PR thickness is around 7 microns.
>
> And also if someone can tell me if Chrome or titanium is a better adhesion
layer for Platinum.
>
> Thanks in Advance,
>
> Forum
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Mentor Graphics Corporation
Addison Engineering