MEMSnet Home: MEMS-Talk: PMMA as hard mask
PMMA as hard mask
2009-08-24
renil kumar
2009-08-25
Jie Zou
2009-08-25
[email protected]
PMMA as hard mask
renil kumar
2009-08-24
Hi all,
            Can I use PMMA as hard mask during Silicon DRIE. What is the
selectivity between PMMA and Silicon during Bosch process. Any suggestions
regarding this will be grately appreciated.

renil