MEMSnet Home: MEMS-Talk: PMMA as hard mask
PMMA as hard mask
2009-08-24
renil kumar
2009-08-25
Jie Zou
2009-08-25
[email protected]
PMMA as hard mask
Jie Zou
2009-08-25
huge. Even more than 100 if you choose some recipes aiming at fast etching.

On Mon, Aug 24, 2009 at 7:20 AM, renil kumar wrote:
> Hi all,
>             Can I use PMMA as hard mask during Silicon DRIE. What is the
selectivity between PMMA and Silicon during Bosch process. Any suggestions
regarding this will be grately appreciated.
>
> renil

*  Zou Jie (Jay)
*  Department of Physics
*  University of Florida
*  Tel: +1-352-846-8018
*  Email: [email protected]
*  Homepage: http://plaza.ufl.edu/zoujie/
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
The Branford Group
Harrick Plasma, Inc.