Plasma bonding works.  Bill Moffat

-----Original Message-----
From: [email protected] [mailto:mems-
[email protected]] On Behalf Of Miyakawa,
Natsuki
Sent: Tuesday, May 18, 2010 11:43 AM
To: General MEMS discussion
Subject: [mems-talk] SiO2-Glass anodic bonding

Dear all,

Is it possible to bond thermally oxidized Si-Wafer (wafer back side is free of
oxide) with glass-wafer anodically? If yes, with which parameter? I tried 500°C
/ 600V (which work well for Si-glass anodic bonding), but it didn't work.

Thank you!

Natsuki
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMStaff Inc.