SiO2-Glass anodic bonding
Khaldoun Halalo
2010-05-19
Hello all,

Can you tell me more about plasma bonding. I couldn't find literature about
it. Is it the same like plasma enhanced optical contacting (bonding)?

thnx
Khaldoun Halalo


>
> -------- Original-Nachricht --------
> Datum: Tue, 18 May 2010 12:29:48 -0700
> Von: "Bill Moffat" 
> An: "General MEMS discussion" 
> Betreff: Re: [mems-talk] SiO2-Glass anodic bonding
>
>             Plasma bonding works.  Bill Moffat

Gruß

Khaldoun Halalo
[email protected]

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Mentor Graphics Corporation