solvent that only removes shipley1813
2010-11-05
LEE
2010-11-05
Marcel Spurny
2010-11-05
Alex Mellnik
solvent that only removes shipley1813
LEE
2010-11-05
I am looking for a high selective solvent, which only remove shipley1813
with no affect on AZ4620. Does anybody use it before?

Btw, Does shipley 1813 stick well with SU-8?

Thanks very much!