MEMSnet Home: MEMS-Talk: solvent that only removes shipley1813
solvent that only removes shipley1813
2010-11-05
LEE
2010-11-05
Marcel Spurny
2010-11-05
Alex Mellnik
solvent that only removes shipley1813
Marcel Spurny
2010-11-05
Try acetone, depending on how you've treated your az it should do the job.

Cheers,
Marcel


Am 05/11/2010 16:01, schrieb LEE:
> I am looking for a high selective solvent, which only remove
> shipley1813 with no affect on AZ4620. Does anybody use it before?
>
> Btw, Does shipley 1813 stick well with SU-8?
>
> Thanks very much!
>
> LEE

Marcel Spurny, Dipl. Phys. MPhys.
School of Physics&  Astronomy
University of St. Andrews
North Haugh
St. Andrews
KY16 9SS
Fife
Scotland, United Kingdom
Tel.: 01334 467336

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing