Re: Photoresist Tape
1999-05-14
Claude Beaulieu
1999-05-14
Jason Tauscher
1999-05-14
Shile
1999-05-14
Patrick C.P. Cheung
1999-05-15
Ken Westra
1999-05-18
Hubert Lorenz
Re: Photoresist Tape
Claude Beaulieu
1999-05-14
You can use "dry film". This is used in the PC board and flat pannel
display industries. The film is applied on the substrate by lamination.
Dupont is selling this type of material wich is a UV sensitive
negative resist.


At 10:45 AM 5/13/99 -0400, you wrote:
>
>Anyone know of something called photoresist "tape"?  Someone described it
>to me as being patternable photoresist, but in a "tape" solid form instead
>of that of liquid.  Please let me know where it can be purchased, and if
>such a product even exists.  Thanks.
>
>-Angela Rasmussen
>The George Washington University
>The Institute of MEMS and VLSI Technologies
>
>
>
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
University Wafer
The Branford Group