1999-05-14
Dry film resist is used for printed circuit board mfg.  It comes in rolls
~8" and wider.  It is probably limited to relatively large geometrys, as the
resist is ~ a mil or more thick.
-----Original Message-----
From: Angela Rasmussen 
To: [email protected] 
Date: Thursday, May 13, 1999 6:33 PM
Subject: Photoresist Tape


>
>Anyone know of something called photoresist "tape"?  Someone described it
>to me as being patternable photoresist, but in a "tape" solid form instead
>of that of liquid.  Please let me know where it can be purchased, and if
>such a product even exists.  Thanks.
>
>-Angela Rasmussen
>The George Washington University
>The Institute of MEMS and VLSI Technologies
>
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Mentor Graphics Corporation