A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Thin film deposition at room temperature
Thin film deposition at room temperature
2012-08-23
Yingtao Tian
2012-08-23
Alex Mellnik
2012-08-23
Yingtao Tian
2012-08-23
Ruiz, Marcos Daniel (SGNCOE)
2012-08-23
Nabhiraj Yalagoud
2012-08-23
Yingtao Tian
2012-08-23
G. Puebla-Hellmann
2012-08-23
Nabhiraj Yalagoud
2012-08-23
Jesse D Fowler
2012-08-24
Piyush Shah
2012-08-24
Sudhin Thampi
2012-08-24
Rajul Patkar
Thin film deposition at room temperature
Yingtao Tian
2012-08-23
Hi All,

I am trying to get round of how to put a thin film down at room temperature. I
need a localised thin film with following properties:

1. non-transparent
2. as thin as possible - say in the order of few microns
3. easy to remove
4. can be applied at around room temperature

I am thinking of some possible spray, but have not got any clue. I would
appreciate if you have some  interesting idea about it.


Thanks a lot.

Regards,
Yingtao
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Addison Engineering
Nano-Master, Inc.