MEMSnet Home: MEMS-Talk: Thin film deposition at room temperature
Thin film deposition at room temperature
2012-08-23
Yingtao Tian
2012-08-23
Alex Mellnik
2012-08-23
Yingtao Tian
2012-08-23
Ruiz, Marcos Daniel (SGNCOE)
2012-08-23
Nabhiraj Yalagoud
2012-08-23
Yingtao Tian
2012-08-23
G. Puebla-Hellmann
2012-08-23
Nabhiraj Yalagoud
2012-08-23
Jesse D Fowler
2012-08-24
Piyush Shah
2012-08-24
Sudhin Thampi
2012-08-24
Rajul Patkar
Thin film deposition at room temperature
Nabhiraj Yalagoud
2012-08-23
Hello,
What film on what substrate you want?
Nabhiraj

On Thu, Aug 23, 2012 at 8:41 PM, Yingtao Tian  wrote:

> Hi All,
>
> I am trying to get round of how to put a thin film down at room
> temperature. I need a localised thin film with following properties:
>
> 1. non-transparent
> 2. as thin as possible - say in the order of few microns
> 3. easy to remove
> 4. can be applied at around room temperature
>
> I am thinking of some possible spray, but have not got any clue. I would
> appreciate if you have some  interesting idea about it.
>
>
> Thanks a lot.
>
> Regards,
> Yingtao
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
MEMStaff Inc.