MEMSnet Home: MEMS-Talk: SU8 for Au Plating
SU8 for Au Plating
2013-03-19
Jocelyn Ng
2013-04-04
Kevin Nichols
2013-04-04
Michael Martin
2013-04-03
André Bödecker
2013-04-03
Bill Moffat
2013-04-04
Jocelyn Ng
2013-04-04
André Bödecker
SU8 for Au Plating
Jocelyn Ng
2013-04-04
Dear André,

Because previously I was using THB120N which had obsoleted, and SU8 was
suggested as replacement. I already have photo masks for negative resist,
therefore I continue to do evaluation for SU8.
I post exposé bake at 95C for 120S, while my plating temp is at ~45C for 24min.
I thought this plating temp is not high enough to harden the SU8?

Thank you.

Best Regards,
Jocelyn

On 3 Apr, 2013, at 16:52, André Bödecker  wrote:

> Dear Jocelyn,
>
>
>
> what is the reason for you to use SU-8? This resist is designated as a
> permanent resist so it is quite unsuitable for plating processes in the case
> you want to remove it afterwards. For such applications I would recommend a
> normal positive resist.
>
>
>
> Best regards,
>
> André Bödecker
>
>
>
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
University Wafer
MEMS Technology Review