SU8 for Au Plating
André Bödecker
2013-04-04
Dear Jocelyn,



I think the PEB temperature is o.k. (we use similar temperatures following
the datasheet). The crosslinking starts widely at that temperature but is
not really finished before you make a hard bake. If you want to remove the
resist after plating I would prefer the negative working plating resists AZ
15 nXT or AZ 125 nXT:

http://www.microchemicals.com/products/photoresists.html



Best regards,



Mit freundlichem Gruß



André Bödecker



Institut für Mikrosensoren, -aktoren und -systeme

Universität Bremen Fachbereich 1

Otto-Hahn-Allee1

28359 Bremen

Tel: 0421 218 62596



_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
MEMStaff Inc.