MEMSnet Home: MEMS-Talk: lift-off
lift-off
2001-12-07
Rajsekhar Popuri
2001-12-07
Michael Pedersen
2001-12-07
Rick Williston
2001-12-07
Bruno Wacogne
2001-12-10
Vladimir Gelfandbein
2001-12-07
[email protected]
lift-off
Michael Pedersen
2001-12-07
I suspect you need an adhesion layer. A thin layer of Cr or Ti/W should
work well for you.

-Michael P.

Rajsekhar Popuri wrote:

> Hello,
>
> I am trying to do a lift-off.I sputter coated gold-palladium of 2000A
> thickness on a glass wafer.When i tried to do a lift-off with
> acetone-methanol,gold-palladium layer was completely peeled off the
> glass wafer.Can anyone tell me the reason for this and suggest a
> suitable process to do a lift-off with gold-palladium.
>
> Thanks in advance
> Rajsekhar.
>
>
>
>
> _________________________________________________________________
> Get your FREE download of MSN Explorer at http://explorer.msn.com/intl.asp
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/


--
MEMS-Exchange
Corporation for National Research Initiatives
1895 Preston White Drive, Ste. 100
Reston, VA 20191-5434

Phone:  703-262-5342
Fax:    703-262-5367
e-mail:
[email protected]
Please visit us @: www.mems-exchange.org

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.