lift-off
Bruno Wacogne
2001-12-07
Hi,

Usually, gold does not adhere to the glass. A thin Cr layer is required
between the glass wafer and the gold layer in order to improve the adhesion
of gold.

good luck
Bruno


At 10:09 07/12/2001 -0500, you wrote:
>Hello,
>
>I am trying to do a lift-off.I sputter coated gold-palladium of 2000A
>thickness on a glass wafer.When i tried to do a lift-off with
>acetone-methanol,gold-palladium layer was completely peeled off the glass
>wafer.Can anyone tell me the reason for this and suggest a suitable process
>to do a lift-off with gold-palladium.
>
>Thanks in advance
>Rajsekhar.
>
>
>
>
>_________________________________________________________________
>Get your FREE download of MSN Explorer at http://explorer.msn.com/intl.asp
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.mems-exchange.org/
>
***********************************************
*                                             *
*   Dr Bruno Wacogne                          *
*   Laboratoire d'Optique P.M. Duffieux       *
*   Faculti des Sciences et des Techniques    *
*   Route de Gray                             *
*   25030 Besangon cedex                      *
*                                             *
*   tel  (++33) 3 81 66 64 25                 *
*   fax  (++33) 3 81 66 64 23                 *
*   mel  [email protected]         *
*                                             *
* http://imfc.univ-fcomte.fr/lopmd/index.html *
* http://imfc.univ-fcomte.fr/                 *
*                                             *
***********************************************

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
MEMS Technology Review
The Branford Group