MEMSnet Home: MEMS-Talk: Metallisation of deep via
Metallisation of deep via
2002-04-23
Han Chong
2002-04-24
[email protected]
2002-04-24
Tao Wang
Metallisation of deep via
Han Chong
2002-04-23
Hi,

Is there any method can metallise a through hole of 20
microns in diameter and 300 microns deep?

thanks

regards

Han Chong
RMIT University
Australia