MEMSnet Home: MEMS-Talk: Metallisation of deep via
Metallisation of deep via
2002-04-23
Han Chong
2002-04-24
[email protected]
2002-04-24
Tao Wang
Metallisation of deep via
Tao Wang
2002-04-24
Electrodeposition works perfectly.

tao

From:     Han Chong @memsnet.org on
04/24/2002 03:37 AM GMT
Please respond to [email protected]
Sent by:  [email protected]

To:  [email protected]
cc:   (bcc: Tao Wang/twang/LSU)

Subject:  [mems-talk] Metallisation of deep via



Hi,

Is there any method can metallise a through hole of 20
microns in diameter and 300 microns deep?

thanks

regards

Han Chong
RMIT University
Australia
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
University Wafer
Process Variations in Microsystems Manufacturing
MEMS Technology Review