Aluminum etch problem
Any MEMS Gyro to buy?
2002-07-23
Robert Dean
2002-07-23
Robert Dean
2002-07-24
Xuchun Liu
non-shrinking epoxy
2002-07-25
Yu Chang
2002-07-24
Greg Miller
2002-07-24
[email protected]
2002-07-24
Bill Moffat
Any MEMS Gyro to buy?
Robert Dean
2002-07-23
Max,

Hi.  Analog Devices sells them.  They are not on their web site, but they
are available.  I have used several of them.  They are quite good.

Sincerely,

Robert Dean

At 11:23 AM 7/23/02 -0300, you wrote:
>Hello, my friends.
>
>If anyone happen to know a commercially available MEMS gyroscope please let
>me know. With our limited resources, I'm not able to find gyros other than
>for defense purposes.
>
>Thanks so much!
>
>Max
>_________________________________________________
>
>Maximiliano Fischer
>Eng. MSc. Aero & Astro
>MEMS Group CNEA
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
Nano-Master, Inc.
Harrick Plasma, Inc.