Aluminum etch problem
Any MEMS Gyro to buy?
2002-07-23
Robert Dean
2002-07-23
Robert Dean
2002-07-24
Xuchun Liu
non-shrinking epoxy
2002-07-25
Yu Chang
2002-07-24
Greg Miller
2002-07-24
[email protected]
2002-07-24
Bill Moffat
Aluminum etch problem
Greg Miller
2002-07-24
You can used MIF327 works quite well for removing Al depending on how
thick - it is very slow.
Thanks,

Greg Miller
KVH Industries
Email: [email protected]


-----Original Message-----
From: Robert Dean [mailto:[email protected]]
Sent: Tuesday, July 23, 2002 5:20 PM
To: [email protected]
Subject: [mems-talk] Aluminum etch problem


>Hello,

I have a fab process where I need to pattern a thin aluminum layer that
has
been deposited on copper.  Unfortunately, the aluminum etch I have is
PAE,
which also etches copper.  Any suggestions other than Cl2 RIE?  The
aluminum layer is used as a mask for a later processing step and could
be
changed to another metal.

Sincerely,

Robert Dean

Research Associate IV
Center for Advanced Vehicle Electronics
Auburn University
200 Broun Hall
Auburn, AL 36849

Voice: 334-844-1838
Fax:   334-844-1898
Email: [email protected]
Web: http://www.eng.auburn.edu/~rdean/index.htm
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
MEMS Technology Review
The Branford Group