MEMSnet Home: MEMS-Talk: Nickel etchant
Nickel etchant
2002-09-09
Phaneendra Medida(fabbi)
2002-09-09
David Nemeth
2002-09-09
Neal Ricks
2002-09-10
David Nemeth
2002-09-09
Neal Ricks
2002-09-09
Kishan Gupta
2002-09-10
Neal Ricks
2002-09-10
Kishan Gupta
2002-09-10
Eric Sanjuan
polymer materials
2002-09-11
Adrian Stoian
Nickel etchant
Neal Ricks
2002-09-09
David,
The KI/I mix is a Gold etchant, so could the effect you've seen be the result of
access to the Gold (i.e. pinholing, lift-off, or undercut of the Nickel), rather
than an electrochemical effect?
Neal
 David Nemeth wrote:In my experience, this solution will not attack Nickel that
is not in
contact with another metal. It will aggressively attack nickel that is
sandwiched between two layers of gold (don't ask me why - go ask an
electrochemist). It will sometimes attack nickel that is on top of gold,
depending on the deposition method of the Nickel.

David Nemeth
Senior Process Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA
Ph: (703) 961-9573 x206
Fax:(703) 961-9576

-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of Phaneendra Medida(fabbi)
Sent: Monday, September 09, 2002 2:47 PM
To: [email protected]
Subject: [mems-talk] Nickel etchant


Does this solution (KI(Potassium iodide)+I2(Iodine)+Water) Etch Nickel?

Fabbi.
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


---------------------------------
Do You Yahoo!?
Yahoo! Finance - Get real-time stock quotes
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
Addison Engineering
MEMStaff Inc.