MEMSnet Home: MEMS-Talk: Nickel etchant
Nickel etchant
2002-09-09
Phaneendra Medida(fabbi)
2002-09-09
David Nemeth
2002-09-09
Neal Ricks
2002-09-10
David Nemeth
2002-09-09
Neal Ricks
2002-09-09
Kishan Gupta
2002-09-10
Neal Ricks
2002-09-10
Kishan Gupta
2002-09-10
Eric Sanjuan
polymer materials
2002-09-11
Adrian Stoian
Nickel etchant
Eric Sanjuan
2002-09-10
hello All,
Does anyone know of a nickel etchant that doesn't etch copper or has very
good selectivity to copper? Would you recommend a book that has an extensive
collection of wet etchants (Similar to Vossen and Kern but more up to date)?
                                                                    thx,

eric



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
The Branford Group
University Wafer
Addison Engineering