MEMSnet Home: MEMS-Talk: Ceramic dicing blade
Ceramic dicing blade
2002-12-26
[email protected]
2002-12-30
RobDavis
Ceramic dicing blade
[email protected]
2002-12-26
Dear friends,

    I am looking for a diamond sawing blade to dice up the
ceramic (alumina) wafers. I was using the disco diamond
blade before, but the result wasn't good (that blade dies
out very fast). Does anybody has the experience of dicing up
the ceramic wafers? Does anybody know which blade
manufacturers are good at ceramic dicing? My wafer sawing
machine is DISCO DAD341. I need a ceramic dicing blade which
is durable, accurate width tolorance and low chipping rate.
Thanks!

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
Mentor Graphics Corporation
University Wafer