MEMSnet Home: MEMS-Talk: Ceramic dicing blade
Ceramic dicing blade
2002-12-26
[email protected]
2002-12-30
RobDavis
Ceramic dicing blade
RobDavis
2002-12-30
Diamond cutting has several factors to consider.....most good, high quality
diamond cutting tools are made using electroless or electrolytic deposited
nickel and diamond slurry.  The corners of the diamond particles need to
stand above the nickel surface. During cutting the diamond edges need to be
re-fractured using an special stone.  Optimum cutting rates use a number of
factors.  The type of blade, taper and thickness are all important, but when
cutting, the diamond saw and work pieces needs to be cooled with water (the
water washes the debris from the low points).  Some of the best diamond
cutting technology is the slicing of silicon logs into wafers.
Rob

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of [email protected]
Sent: Thursday, December 26, 2002 4:24 AM
To: [email protected]
Cc: [email protected]
Subject: [mems-talk] Ceramic dicing blade


Dear friends,

    I am looking for a diamond sawing blade to dice up the
ceramic (alumina) wafers. I was using the disco diamond
blade before, but the result wasn't good (that blade dies
out very fast). Does anybody has the experience of dicing up
the ceramic wafers? Does anybody know which blade
manufacturers are good at ceramic dicing? My wafer sawing
machine is DISCO DAD341. I need a ceramic dicing blade which
is durable, accurate width tolorance and low chipping rate.
Thanks!

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMS Technology Review
University Wafer
Process Variations in Microsystems Manufacturing