crucible for Ti
2003-12-22
"Lee, Duhyun"
2003-12-23
[email protected]
2003-12-23
Blunier, Stefan
2003-12-23
[email protected]
crucible for Ti
[email protected]
2003-12-23
We have been evaporating Ti in our system for 3 years without any crucible
and any problems. I guess it depend upon what purity you are needing - we
are not worried as we just use as a seed layer

Mark Leonard


On Mon, 22 Dec 2003 17:24:56 -1200, "Lee, Duhyun"  wrote:

>
>
> <!--startrecall--><img
> src="http://mail.skku.edu/mail/write/mail_recall.php?
[email protected]"><!--
endrecall-->
>
> What kind of crucible can I use for e-beam evaporation of Ti?
> As far as I know, TiC is recommended, but I don't have it.
>
> I have Al2O3, Mo, W, and graphite crucibles.
>
> please advice me...
>
>
> Lee, Duhyun
>
> ========================================
> [email protected]
> Technology Innovation Center(TIC)
> Dep. of Advanced Materials Eng.
> Sungkyunkwan University, KOREA
> Tel +82-31-290-5645
> Fax +82-31-290-5644
> ========================================
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your
> list
> options, visit
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing
> services.
> Visit us at http://www.memsnet.org/
>

________________________________________________________________

DISCLAIMER:

This e-mail and any files transmitted with it are confidential
and intended solely for the use of the individual or entity to
whom it is addressed.  If you are not the intended recipient
you are prohibited from using any of the information contained
in this e-mail.  In such a case, please destroy all copies in
your possession and notify the sender by reply e-mail.  Heriot
Watt University does not accept liability or responsibility
for changes made to this e-mail after it was sent, or for
viruses transmitted through this e-mail.  Opinions, comments,
conclusions and other information in this e-mail that do not
relate to the official business of Heriot Watt University are
not endorsed by it.
________________________________________________________________


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
University Wafer
The Branford Group