crucible for Ti
[email protected]
2003-12-23
 No crucible is needed.  Just drop your Ti in the copper pocket.

Brent Garber

Original Message:
-----------------
From: "Lee, Duhyun" [email protected]
Date: Mon, 22 Dec 2003 17:24:56 -1200
To: [email protected]
Subject: [mems-talk] crucible for Ti






What kind of crucible can I use for e-beam evaporation of Ti?
As far as I know, TiC is recommended, but I don't have it.

I have Al2O3, Mo, W, and graphite crucibles.

please advice me...


Lee, Duhyun

========================================
[email protected]
Technology Innovation Center(TIC)
Dep. of Advanced Materials Eng.
Sungkyunkwan University, KOREA
Tel +82-31-290-5645
Fax +82-31-290-5644
========================================
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

--------------------------------------------------------------------
mail2web - Check your email from the web at
http://mail2web.com/ .




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Harrick Plasma, Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing