crucible for Ti
2003-12-22
"Lee, Duhyun"
2003-12-23
[email protected]
2003-12-23
Blunier, Stefan
2003-12-23
[email protected]
crucible for Ti
Blunier, Stefan
2003-12-23
Hi Duhyun
According to the "Edwards" catalogue carbon crucibles are recommended
for Ti.
greetings
Stefan

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On
Behalf Of "Lee, Duhyun"
Sent: Dienstag, 23. Dezember 2003 06:25
To: [email protected]
Subject: [mems-talk] crucible for Ti




<!--startrecall--><img
src="http://mail.skku.edu/mail/write/mail_recall.php?f_headindex=15
[email protected]"><!--endrecall-->

What kind of crucible can I use for e-beam evaporation of Ti? As far as
I know, TiC is recommended, but I don't have it.

I have Al2O3, Mo, W, and graphite crucibles.

please advice me...


Lee, Duhyun

========================================
[email protected]
Technology Innovation Center(TIC)
Dep. of Advanced Materials Eng.
Sungkyunkwan University, KOREA
Tel +82-31-290-5645
Fax +82-31-290-5644
========================================
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
MEMStaff Inc.
Harrick Plasma, Inc.
Nano-Master, Inc.