MEMSnet Home: MEMS-Talk: Does concentrated HF etch Au
Does concentrated HF etch Au
2004-02-16
li Yu
2004-02-16
David Nemeth
2004-02-16
Jing Liu
2004-02-16
Tres Brooks
2004-02-16
[email protected]
Does concentrated HF etch Au
li Yu
2004-02-16
I want to put a wafer with 2000A Au in 49% HF for 30 minute, Is that Ok? Thanks
in advance.
 Lili


---------------------------------
Do you Yahoo!?