MEMSnet Home: MEMS-Talk: Does concentrated HF etch Au
Does concentrated HF etch Au
2004-02-16
li Yu
2004-02-16
David Nemeth
2004-02-16
Jing Liu
2004-02-16
Tres Brooks
2004-02-16
[email protected]
Does concentrated HF etch Au
Jing Liu
2004-02-16
Based on former experice, I think that should be fine.

Jing


On Sun, 15 Feb 2004, li Yu wrote:

> I want to put a wafer with 2000A Au in 49% HF for 30 minute, Is that Ok?
Thanks in advance.
>  Lili
>
>
> ---------------------------------
> Do you Yahoo!?
> Yahoo! Finance: Get your refund fast by filing online
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
University Wafer
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics