Does concentrated HF etch Au
Tres Brooks
2004-02-16
You should be fine.  If there are any pin holes in the gold then the HF will
find a way to the substrate but if your coating is uniform you should have no
problems.

Tres

-----Original Message-----
From: li Yu [mailto:[email protected]]
Sent: Sunday, February 15, 2004 9:14 PM
To: [email protected]
Subject: [mems-talk] Does concentrated HF etch Au


I want to put a wafer with 2000A Au in 49% HF for 30 minute, Is that Ok? Thanks
in advance.
 Lili


---------------------------------
Do you Yahoo!?
Yahoo! Finance: Get your refund fast by filing online
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
The Branford Group
Addison Engineering